NANOINDENTATION RESPONSE OF ITO FILM

Nanoindentation response of ITO film

 

Nanoindentation response of ITO film, Maurya Sandeep Pradeepkumar, K. P. Sibin, Niharika Swain, N. Sridhara, Arjun Dey, H. C. Barshilia, A. K. Sharma, Ceramics International, 41 (2015) 8223-8229, doi:10.1016/j.ceramint.2015.02.090 